What went wrong, and the fix — from Fabrication Bench’s guides
| went wrong | the fix |
|---|---|
| Corners lift | Wash the plate, level, slow the first layer |
| Stringing | Dry the spool at the preset |
| Hissing at the nozzle | Moisture — dry, bag warm |
| Ran out | Weigh the spool: 2.98 g/m for 1.75 mm PLA |
| went wrong | the fix |
|---|---|
| Scorches | E = W·(p/100)·N/v — reduce, increase speed |
| Didn’t cut through | Add passes or slow |
| Edge rough | Check the data sheet |